反応式
[CH3:1][CH2:2][CH2:3][CH2:4][CH:5]([CH2:8][CH2:9][CH:10](OS([O-])(=O)=O)[CH2:11][CH:12]([CH3:14])C)[CH2:6]C.[Na+]>O>[CH2:1]=[CH:2][CH:3]=[CH2:4].[CH2:14]=[CH:12][C:11]1[CH:6]=[CH:5][CH:8]=[CH:9][CH:10]=1参加物
3
実験手順
The material was prepared by dispersing 0.80 g Tergitol TMN-06 in 1481 g deionized water with an air mixer. To this was then added 1159 g of ground crystalline silicotitanate (150 g, 13.0% solids) (IONSIV IE 910) with agitation. Slowly to this was added 150.1 g Goodrite 1800×73 (39% solids, 58.5 g) with stirring. This mixture was mixed for 1 hour with an air mixer. The slurry was spray dried using a Niro Atomizer, (Serial number #2402) at 35 mL/min. Spray drying conditions were as follows:
後処理
- customThe material was prepared
- additionThis mixture was mixed for 1 hour with an air mixer
- customdried
- customSpray drying conditions
出典と根拠
- ORDレコード
- ord-e2d357fa244044eeb976b4fe3b6f5260
- 出典データセット
- uspto-grants-1999_11
- 特許番号
- US05989434
関連ノート
読み込み中…