ホームMCPワークベンチSkills
ホームワークベンチ通知マイページ
llms.txt · MCPガイドプライバシーポリシー · 利用規約 · サポートv1.8.3
  1. ホーム
  2. /反応

2-Mercaptoethanol → Acrylic acid vinylpyrrolidone

HRID 2169659
印刷

反応式

HRID 2169659 の反応式
[CH:1]([N:3]1[CH2:7][CH2:6][CH2:5][C:4]1=[O:8])=[CH2:2].[C:9]([OH:13])(=[O:12])[CH:10]=[CH2:11].N(C(C1NCCN=1)(C)C)=NC(C1NCCN=1)(C)C.SCCO>CC(C)=O.O.CS(C)=O>[CH:1]([N:3]1[CH2:7][CH2:6][CH2:5][C:4]1=[O:8])=[CH2:2].[C:9]([OH:13])(=[O:12])[CH:10]=[CH2:11]
参加物実験手順後処理出典と根拠反応ノート

参加物

8

反応物 4

HCID 15672-MercaptoethanolHCID 6581Acrylic AcidHCID 6917N-vinyl-2-pyrrolidoneHCID 887152,2'-Azobis(2-(2-imidazolin-2-yl)propane)

生成物 1

HCID 197163Acrylic acid vinylpyrrolidone

試薬・触媒・溶媒 3

HCID 180Acetone溶媒2 回
HCID 679
Dimethyl Sulfoxide
溶媒
HCID 962Water溶媒

実験手順

In a 500 mL three-necked flask, N-vinylpyrrolidone (33.34 g, 0.30 mol), acrylic acid (43.24 g, 0.60 mol), dimethyl sulfoxide (307.08 g), a polymerization initiator VA-061 (Wako Pure Chemical Industries, Ltd., 0.1408 g, 0.562 mmol) and 2-mercaptoethanol (43.8 μL, 0.63 mmol) were charged, and then equipped with a three-way stop-cock, a reflux condenser tube, a thermometer and a mechanical stirrer. The concentration of the monomer was 20% by weight. After degassing inside the three-necked flask using a vacuum pump and repeating replacement by argon three times, stirring was carried out at 50° C. for 0.5 hours, followed by temperature rise to 70° C. and further stirring for 6.5 hours. After completion of the polymerization, the polymerization reaction solution was cooled to room temperature and 100 mL of water was added, and then the solution was poured into 500 mL of acetone and the mixed solution was left to stand overnight. On the next day, 200 mL of acetone was further added and then the supernatant was removed by decantation. The obtained solid component was washed seven times with acetone/water (=700 mL/100 mL). The solid component was dried overnight by a vacuum drying oven at 60° C. Liquid nitrogen was charged and the solid component was crushed by a spatula, and then dried by a vacuum drying oven at 60° C. for 3 hours. The thus obtained copolymer had a molecular weight of Mn: 65 kD, Mw: 202 kD (Mw/Mn=3.1).

後処理

  1. customequipped with a three-way
  2. customAfter degassing inside the three-necked flask
  3. customfollowed by temperature rise to 70° C.
  4. stirringfurther stirring for 6.5 hours
  5. customAfter completion of the polymerization
  6. customthe polymerization reaction solution
  7. waitthe mixed solution was left
  8. waitto stand overnight
  9. customthe supernatant was removed by decantation
  10. washThe obtained solid component was washed seven times with acetone/water (=700 mL/100 mL)
  11. customThe solid component was dried overnight by a vacuum
  12. customdrying oven at 60° C
  13. additionLiquid nitrogen was charged
  14. customthe solid component was crushed by a spatula
  15. customdried by a vacuum
  16. customdrying oven at 60° C. for 3 hours

出典と根拠

ORDレコード
ord-71c50c83797147b98eadb5532af70a2a
出典データセット
uspto-grants-2015_06
DOI
10.6084/m9.figshare.5104873.v1
特許番号
US09046644B2

反応ノート

このページの内容参加物実験手順後処理出典と根拠反応ノート