1-Butanol → Trimellitic anhydride

HRID 237188

反応式

HRID 237188 の反応式
[CH2:1](O)[CH3:2].CC([O:9][C:10](C)=[O:11])COC.CCO[Si]([O:23][CH2:24][CH3:25])(OCC)OCC.[N+]([O-])(O)=[O:27].[CH2:30]([OH:34])[CH2:31][CH2:32][CH3:33]>O>[CH:1]1[C:31]([C:30]([OH:27])=[O:34])=[CH:32][C:33]2[C:10]([O:11][C:24](=[O:23])[C:25]=2[CH:2]=1)=[O:9]

参加物

7

反応条件

温度
81 °C

実験手順

To the solvents of 60 g ethanol and 30 g PGMEA, 33.33 g TEOS, 5.71 g VTEOS and 2.40 g PTEOS monomers were individually added. While stirring a mixture of 1.13 g 0.1N nitric acid and 18.92 g water was poured, the reaction mixture was heated to reflux at 81° C. for 4 hours before cooling down. 8.84 g butanol was added to the reaction mixture and stirred at room temperature overnight. The resulting polymer was measured to have a molecular weight of Mn=1121 amu, Mw=1723 amu analyzed using the same GPC system as mentioned above.

後処理

  1. additionwas poured
  2. temperaturethe reaction mixture was heated
  3. temperaturebefore cooling down
  4. stirringstirred at room temperature overnight

出典と根拠

ORDレコード
ord-31631c81520743ecb2d1a43171b221ea
出典データセット
uspto-grants-2014_02
特許番号
US08642246B2