실험 절차

Polymerization of styrene with the system NaNH2 and triethylene glycol monobutyl ether. Polymerization is allowed to proceed from 8.32 g (8·10-22 mole) of styrene in in 30 cc THF in the presence of 0.98 g (25·10-3 mole) of sodium amide and 1.71 g (8.3·10-3 mole) of triethylene glycol monobutyl ether. The reaction mixture which is obtained prior to the addition of the monomer has a yellow color which is more pronounced than that obtained with diethylene glycol monoethyl ether, contrary to the results which have been obtained with glycol monomethyl ether. At the end of four hours, a polymer is obtained in 50% yield, with Mn=8500.

후처리

  1. customPolymerization
  2. customThe reaction mixture which is obtained
  3. additionto the addition of the monomer

출처 및 근거

ORD 기록
ord-ee1cd658a5b4488b9bdfd053b4ca7193
출처 데이터셋
uspto-grants-1981_03
특허 번호
US04254247

연결된 노트

불러오는 중…