To the boron carbide powder, 14.5 mol % of the submicron-size or nano-size titanium dioxide powder and 21.5 mol % of carbon black were incorporated, and using a methanol solvent, mixing was carried out by a planetary ball mill made of silicon carbide (SiC) at a rotational speed of 270 rpm for 1 hour, followed by drying by a evaporator and further by drying at 150° C. for 24 hours. Then, the mixture was sieved through a sieve with an opening of 250 μm to obtain a boron carbide-titanium dioxide-carbon mixed powder.
후처리
- additionmixing
- customby drying by a evaporator
- customfurther by drying at 150° C. for 24 hours
- filtrationThen, the mixture was sieved through a sieve with an opening of 250 μm