[Na:1].[C:2]([OH:7])(=[O:6])[C:3]([CH3:5])=[CH2:4].[CH2:8]1[O:10][CH2:9]1.[CH2:11]=[CH:12][C:13]1[CH:18]=[CH:17][CH:16]=[CH:15][CH:14]=1.[C:19]([OH:24])(=[O:23])[C:20]([CH3:22])=[CH2:21].S(OOS([O-])(=O)=O)([O-])(=O)=O.[NH4+].[NH4+]>O>[CH2:11]=[CH:12][C:13]1[CH:18]=[CH:17][CH:16]=[CH:15][CH:14]=1.[C:2]([OH:7])(=[O:6])[C:3]([CH3:5])=[CH2:4].[Na:1].[C:19]([OH:24])(=[O:23])[C:20]([CH3:22])=[CH2:21].[CH2:9]1[O:10][CH2:8]1참가 물질
실험 절차
A reaction vessel equipped with a stirring rod and a thermometer was charged with 683 parts by mass of water, 11 parts by mass of a sodium salt of sulfuric acid ester of methacrylic acid-ethylene oxide adduct (ELEMINOL RS-30, manufactured by Sanyo Chemical Industries, Ltd.), 138 parts by mass of styrene, 138 parts by mass of methacrylic acid, and 1 part by mass of ammonium persulfate, and the resulting mixture was stirred for 15 minutes at 400 rpm to thereby prepare a white emulsion. The obtained emulsion was heated until the internal system temperature reached 75° C., and then was allowed to react for 5 hours. To the resultant, 30 parts by mass of a 1% by mass ammonium persulfate aqueous solution was further added, and the resulting mixture was aged for 5 hours at 75° C., to thereby obtain an aqueous dispersion liquid of a vinyl resin (a copolymer of styrene/methacrylic acid/a sodium salt of sulfuric acid ester of methacrylic acid-ethylene oxide adduct), i.e. Particle Dispersion Liquid 1.
후처리
- customA reaction vessel equipped with a stirring rod
- customto thereby prepare a white emulsion
- temperatureThe obtained emulsion was heated until the internal system temperature
- customreached 75° C.
- customto react for 5 hours
- waitthe resulting mixture was aged for 5 hours at 75° C.