[C:1]([O:6][CH2:7][CH2:8][CH2:9][Si:10]([O:15][CH3:16])([O:13][CH3:14])[O:11][CH3:12])(=[O:5])[C:2]([CH3:4])=[CH2:3].[C:17]([O:22][CH3:23])(=[O:21])[C:18]([CH3:20])=[CH2:19].N(C(C)(C)C#N)=NC(C)(C)C#N>C1(C)C(C)=CC=CC=1>[C:1]([O:6][CH2:7][CH2:8][CH2:9][Si:10]([O:15][CH3:16])([O:11][CH3:12])[O:13][CH3:14])(=[O:5])[C:2]([CH3:4])=[CH2:3].[C:17]([O:22][CH3:23])(=[O:21])[C:18]([CH3:20])=[CH2:19]참가 물질
5
반응 조건
- 온도
- 100 °C
실험 절차
An undercoating material was prepared as follows. A mixture of 20 parts gamma-methacryloxypropyltrimethoxysilane, 80 parts methyl methacrylate, 100 parts xylene, and 1.0 part azobisisobutyronitrile was mixed and then heated at 100° C. for 3 hours to give gamma-methacryloxypropyltrimethoxysilane-methyl methacrylate copolymer. Xylene was added to this copolymer to prepare an undercoating material having 40 percent solids and a viscosity of 150 cP.
후처리
- customAn undercoating material was prepared
- additionwas mixed
출처 및 근거
- ORD 기록
- ord-dc9a556e96bc494d975002d8be24b594
- 출처 데이터셋
- uspto-grants-1988_08
- 특허 번호
- US04761312
연결된 노트
불러오는 중…