홈MCPSkills워크벤치OpenChem
홈워크벤치알림마이페이지
llms.txt · skill.md · MCP 가이드개인정보처리방침 · 이용약관 · 지원v1.8.4
  1. 홈
  2. /반응

Isoprene → Butadiene isoprene styrene

HRID 482561
인쇄

반응식

[CH2:1]=[CH:2][C:3](=[CH2:5])[CH3:4].[CH2:6]=[CH:7][C:8]1[CH:13]=[CH:12][CH:11]=[CH:10][CH:9]=1.[CH2:14]=[CH:15][CH:16]=[CH2:17].C([Li])CCC.[Si](Cl)(Cl)(Cl)Cl>CCCCCC.CO>[CH2:6]=[CH:7][C:8]1[CH:13]=[CH:12][CH:11]=[CH:10][CH:9]=1.[CH2:1]=[CH:2][C:3](=[CH2:4])[CH3:5].[CH2:14]=[CH:15][CH:16]=[CH2:17]
참가 물질실험 절차후처리출처 및 근거반응 노트

참가 물질

8

반응물 5

HCID 6557Isoprene3회HCID 7501Styrene2회HCID 78451,3-Butadiene2회HCID 24816Silicon tetrachlorideHCID 178418339Butyllithium

생성물 1

HCID 21879892Butadiene isoprene styrene

시약·촉매·용매 2

HCID 887
Methanol
용매
HCID 8058Hexane용매2회

실험 절차

In this Example, an isoprene terminated, silicon coupled, styrene/isoprene/butadiene rubber (SIBR) was prepared in a two-reactor (10 liters each) continuous system at about 95° C. A premix containing styrene, isoprene and 1,3-butadiene in hexane was charged into the first polymerization reactor continuously at a rate of about 65.6 grams/minute. The premix monomer solution contained a ratio of styrene to isoprene to 1,3-butadiene of about 10:30:60 and had a total monomer concentration of about 14%. Polymerization was initiated by adding a 0.128M solution of n-butyllithium into the first reactor at a rate of about 0.4 grams per minute. The resulting polymerization medium containing the live ends was continuously pushed into the second reactor where the coupling agent, silicon tetrachloride, (0.025M solution in hexane) was added at a rate of about 0.34 grams/minute. The residence time for both reactors was set at two hours to achieve complete monomer conversion in the first reactor and complete coupling in the second reactor. The polymerization medium was then continuously pushed over to a holding tank containing the shortstop (methanol) and an antioxidant. The resulting polymer cement was then steam stripped and the recovered SIBR was dried in a vacuum oven at about 60° C. The styrene distribution in the SIBR was random since the styrene, isoprene and butadiene monomers were continuously pumped into the reactors. The hexane solvent was evaporated and the resulting coupled SIBR terpolymer recovered by drying in a vacuum oven.

후처리

  1. additionwas charged into the first polymerization reactor continuously at a rate of about 65.6 grams/minute
  2. customPolymerization
  3. customThe resulting polymerization medium
  4. additioncontaining the live ends
  5. additionwas added at a rate of about 0.34 grams/minute
  6. customthe recovered SIBR was dried in a vacuum oven at about 60° C
  7. customThe hexane solvent was evaporated
  8. customrecovered
  9. customby drying in a vacuum oven

출처 및 근거

ORD 기록
ord-3e27efb8548d4bceb4135e94ec77ec49
출처 데이터셋
uspto-grants-1998_08
DOI
10.6084/m9.figshare.5104873.v1
특허 번호
US05798408

반응 노트

이 페이지에서참가 물질실험 절차후처리출처 및 근거반응 노트