홈MCP워크벤치Skills
홈워크벤치알림마이페이지
llms.txt · MCP 가이드개인정보처리방침 · 이용약관 · 지원v1.8.3
  1. 홈
  2. /반응

Styrene → Benzene, ethenyl-, polymer with 1,3-butadiene

HRID 485738
인쇄

반응식

HRID 485738 반응식
[CH2:1]=[CH:2][CH:3]=[CH2:4].[CH2:5]=[CH:6][C:7]1[CH:12]=[CH:11][CH:10]=[CH:9][CH:8]=1.C1C=CC(P(C2C=CC=CC=2)(C2C=CC=CC=2)=O)=CC=1.C([Li])CCC.[C:38]([C:42]1[C:47](C)=[CH:46][CH:45]=[C:44](O)[C:43]=1C(C)(C)C)(C)(C)[CH3:39]>CCCCCC.C(O)(C)C>[CH2:1]=[CH:2][CH:3]=[CH2:4].[CH2:5]=[CH:6][C:7]1[CH:12]=[CH:11][CH:10]=[CH:9][CH:8]=1.[CH2:39]=[CH:38][C:42]1[CH:47]=[CH:46][CH:45]=[CH:44][CH:43]=1
참가 물질실험 절차후처리출처 및 근거반응 노트

참가 물질

9

반응물 5

HCID 7501StyreneHCID 78451,3-ButadieneHCID 13097Triphenylphosphine OxideHCID 3034427Phenol, bis(1,1-dimethylethyl)-4-methyl-HCID 178418339Butyllithium

생성물 2

HCID 7501Styrene수율 19.4%
HCID 62697
Benzene, ethenyl-, polymer with 1,3-butadiene
수율 40.9%

시약·촉매·용매 2

HCID 3776Isopropanol용매HCID 8058Hexane용매

실험 절차

A one gallon stainless steel reactor equipped with a stirrer blade is charged with 95 grams of 1,3-butadiene and 19 grams of styrene in 2,000 grams of n-hexane. One-half millimoles of TPPO are added and the temperature is adjusted to 100° C. One millimole of n-butyllithium is added to the mixture in the reaction vessel. Polymerization is completed within 30 minutes with the final maximum reaction temperature reaching 130° C. After termination of the reaction, 0.5 percent by weight of an antioxidant, di-tert-butyl-p-cresol ("IONOL"), based on the reaction mixture, is added to the mixture which is coagulated in isopropanol and drum dried to remove the solids. The initial monomer charge underwent a 93 percent conversion to form the product butadiene-styrene copolymer containing 40.9 percent of 1,2-microstructure and 19.4 percent of styrene as determined by IR spectroscopy.

후처리

  1. customA one gallon stainless steel reactor equipped with a stirrer blade
  2. customis adjusted to 100° C
  3. customPolymerization
  4. customreaching 130° C
  5. additionis added to the mixture which
  6. customdrum dried
  7. customto remove the solids
  8. additionThe initial monomer charge underwent a 93 percent conversion