[C:1]([O-:20])(=[O:19])[CH2:2][CH2:3][CH2:4][CH2:5][CH2:6][CH2:7][CH2:8][CH2:9][CH2:10][CH2:11][CH2:12][CH2:13]CCCCC.[Al+3].[C:22]([O-])(=[O:40])[CH2:23]CCCCCCCCCCCCCCCC.C([O-])(=[O:60])CCCCCCCCCCCCCCCCC.C([O-])(=O)CCCCCCCCCCCCCCCCC.[Li+]>>[C:13]1(=[O:60])[O:40][CH2:22][CH2:23][O:20][C:1](=[O:19])[CH2:2][CH2:3][CH2:4][CH2:5][CH2:6][CH2:7][CH2:8][CH2:9][CH2:10][CH2:11][CH2:12]1

참가 물질

3

반응 조건

온도
314 °C

실험 절차

A mixed metal catalyst comprised of aluminum stearate and lithium stearate (molar ratio 1:1) was used for the depolymerization. For the reaction aluminum stearate (1.09 gram) and lithium stearate (0.36 gram) were blended in 70 grams poly(ethylene brassylate) at 200° C. The temperature was then raised to 314° C. while maintaining a vacuum of 0.05-0.1 mm Hg. Ethylene brassylate was obtained (40 mls during the first hour) in an 88.9 percent yield. Of the ethylene brassylate recovered, 90 percent of the product was obtained after 2 hours.

후처리

  1. temperaturewhile maintaining a vacuum of 0.05-0.1 mm Hg

출처 및 근거

ORD 기록
ord-0f676f5a41704569b949cc4c945350ba
출처 데이터셋
uspto-grants-1985_02
특허 번호
US04499288

연결된 노트

불러오는 중…