Methyl Methacrylate → Benzene, ethenyl-, polymer with 1,3-butadiene

HRID 890322
인쇄

반응식

HRID 890322 반응식
S([O-])[O-].[Na+].C=O.[Na+].C(N(CC(O)=O)CC(O)=O)CN(CC([O-])=O)CC([O-])=O.[Na+].[Na+].C(OC)(=O)C(C)=C.[CH2:37]=[CH:38][C:39]1[CH:44]=[CH:43][CH:42]=[CH:41][CH:40]=1>>[CH2:37]=[CH:38][CH:39]=[CH2:40].[CH2:37]=[CH:38][C:39]1[CH:44]=[CH:43][CH:42]=[CH:41][CH:40]=1
참가 물질실험 절차후처리출처 및 근거반응 노트

참가 물질

5

반응물 4

HCID 6658Methyl MethacrylateHCID 7501StyreneHCID 13020083EDTA disodium saltHCID 21225536CID 21225536

생성물 1

HCID 62697Benzene, ethenyl-, polymer with 1,3-butadiene

실험 절차

An 8 liter polymerization reactor was charged with 70 parts (dry basis) of the latex of particle size enhanced butadiene-styrene rubber obtained in (2). After elevating the temperature to 60° C. in a nitrogen gas stream with stirring, 0.18 part of formaldehyde sodium sulfoxylate, 0.001 part of ferrous sulfate and 0.004 part of disodium ethylenediaminetetraacetate were added to the reactor. Graft polymerization was then carried out in the same manner as in Example 1 by using 30 parts of a monomer mixture of 14.7 parts of methyl methacrylate and 15.3 parts of styrene. The obtained graft copolymer had an average particle size of 7,800 angstroms and a refractive index of 1.537.

후처리

  1. customto 60° C.
  2. customGraft polymerization

출처 및 근거

ORD 기록
ord-570d81764eb7464885ab03c00bbd91fb
출처 데이터셋
uspto-grants-2006_02
DOI
10.6084/m9.figshare.5104873.v1
특허 번호
US06995197B2

반응 노트

이 페이지에서참가 물질실험 절차후처리출처 및 근거반응 노트