Glycine → Zinc Glycinate

HRID 981681
인쇄

반응식

HRID 981681 반응식
[NH2:1][CH2:2][C:3]([OH:5])=[O:4].[O-2].[Zn+2:7].O>>[Zn+2:7].[NH2:1][CH2:2][C:3]([O-:5])=[O:4].[NH2:1][CH2:2][C:3]([O-:5])=[O:4]
참가 물질실험 절차후처리출처 및 근거반응 노트

참가 물질

4

반응물 3

HCID 750GlycineHCID 962WaterHCID 3007857Zinc Oxide

생성물 1

HCID 151910Zinc Glycinate

실험 절차

Glycine zinc salt was prepared by the following procedure. Glycine (300 g; 4 moles) and 162.8 g (2 moles) of zinc oxide were put in a portable universal mixer and mixed for about 5 minutes. Then 162.8 g (34 moles) of water was added, and the mixing was continued for about 1 hour. Then, the mixture was dried at 110° C. to obtain glycine zinc salt as crystals. The crystals were mechanically pulverized and observed under a scanning electron microscope. When the largest particle among those particles which appeared in the visual field has a particle diameter of 10 micrometer, it was determined that the crystals had been finely pulverized to an average particle diameter of not more than 10 micrometers. The above pulverization to an average particle diameter of not more than 10 micrometers was effected by using a jet pulverizer, and the pulverization was repeated.

후처리

  1. customGlycine zinc salt was prepared by the following procedure
  2. additionmixed for about 5 minutes
  3. customThen, the mixture was dried at 110° C.

출처 및 근거

ORD 기록
ord-d069ad6b2f674bfe957602c9aa3fd67a
출처 데이터셋
uspto-grants-1991_02
DOI
10.6084/m9.figshare.5104873.v1
특허 번호
US04992494

반응 노트