Acrylamide → Isooctyl Acrylate Acrylamide Vinyl Acetate
Reaction equation
[C:1]([O:5][CH2:6][CH2:7][CH2:8][CH2:9][CH2:10][CH:11]([CH3:13])[CH3:12])(=[O:4])[CH:2]=[CH2:3].[C:14]([NH2:18])(=[O:17])[CH:15]=[CH2:16].[C:19]([O:22][CH:23]=[CH2:24])(=[O:21])[CH3:20].C(OOC(=O)C1C=CC=CC=1)(=O)C1C=CC=CC=1>C(OCC)(=O)C.CO.C(OCC)(=O)C.CO>[C:1]([O:5][CH2:6][CH2:7][CH2:8][CH2:9][CH2:10][CH:11]([CH3:13])[CH3:12])(=[O:4])[CH:2]=[CH2:3].[C:14]([NH2:18])(=[O:17])[CH:15]=[CH2:16].[C:19]([O:22][CH:23]=[CH2:24])(=[O:21])[CH3:20]Participants
8
Procedure
The procedures above were repeated this time employing 120.0 g. isooctyl acrylate, 8.0 g. acrylamide, 32.0 g. vinyl acetate, 0.32 g. benzoyl peroxide, 216.0 g. ethyl acetate and 24.0 g. methyl alcohol. The resulting polymer was diluted with the ethyl acetate/methyl alcohol mixture to 21.52% solids. The adhesive polymer had a measured inherent viscosity of 1.40 dl/g in ethyl acetate at a concentration of 0.15 g/dl. Its Brookfield viscosity was 2,300 centipoise.
Sources & evidence
- ORD record
- ord-91961685648c4baf8470fe805f28f874
- Source dataset
- uspto-grants-1993_06
- Patent number
- US05223261
Reaction notes
Loading…