Methyl Methacrylate → HCID 20273141, compound
Reaction equation
[C:1]([O-:6])(=[O:5])[C:2]([CH3:4])=[CH2:3].[CH2:7]([Sn+:11]([CH2:16][CH2:17][CH2:18][CH3:19])[CH2:12][CH2:13][CH2:14][CH3:15])[CH2:8][CH2:9][CH3:10].[C:20]([O:25][CH3:26])(=[O:24])[C:21]([CH3:23])=[CH2:22].C(OOC(=O)C1C=CC=CC=1)(=O)C1C=CC=CC=1>C1(C)C(C)=CC=CC=1>[CH3:26][O:25][C:20](=[O:24])[C:21]([CH3:23])=[CH2:22].[C:1]([O-:6])(=[O:5])[C:2]([CH3:4])=[CH2:3].[CH2:16]([Sn+:11]([CH2:7][CH2:8][CH2:9][CH3:10])[CH2:12][CH2:13][CH2:14][CH3:15])[CH2:17][CH2:18][CH3:19]Participants
5
Reactant 3
Product 1
Reagents, catalysts & solvents 1
Procedure
65 parts tributyl tin methacrylate and 35 parts methyl methacrylate were copolymerised in xylene using benzoyl peroxide initiator by the process described in Example 1 to form a 40 percent solids tributyl tin methacrylate methyl methacrylate copolymer solution. This 40 percent copolymer solution was used in the formulation of Example 5 to replace the copolymer solution of Example 1 and the ingredients were blended to form a paint.
Sources & evidence
- ORD record
- ord-0e0d3fc98ba34bd7b1f7bbf1dce09f16
- Source dataset
- uspto-grants-1980_03
- Patent number
- US04191579