N(C(C)(C)C#N)=NC(C)(C)C#N.[CH2:13]=[CH:14][C:15]1[CH:20]=[CH:19][CH:18]=[CH:17][CH:16]=1.[C:21]([O:26][CH2:27][CH2:28][CH2:29][CH3:30])(=[O:25])[C:22]([CH3:24])=[CH2:23]>>[CH2:13]=[CH:14][C:15]1[CH:20]=[CH:19][CH:18]=[CH:17][CH:16]=1.[C:21]([O:26][CH2:27][CH2:28][CH2:29][CH3:30])(=[O:25])[C:22]([CH3:24])=[CH2:23]Participants
4
Conditions
- Temperature
- 110 °C
Procedure
With the addition of 2,2'-azobisisobutyronitrile, a mixture of styrene and n-butyl methacrylate at a mixing ratio of (75:25) was stirred at temperatures of 100 to 120° C. in order to obtain 43 parts by weight of a styrene-n-butyl methacrylate copolymer. The previously obtained solution was further added dropwise to the above polymerization mixture and the polymerization was allowed to continue for three hours. Thereafter, a solvent component was removed from the above mixture by heating under vacuum.
Sources & evidence
- ORD record
- ord-ab30ceebb68f49f4b5f0e5904e754478
- Source dataset
- uspto-grants-1995_01
- Patent number
- US05380616
Reaction notes
Loading…