HRID2248420

反应详情

EQUATION

反应方程式

HRID 2248420 的结构方程式

AUXILIARIES

试剂、催化剂与溶剂

1

CONDITIONS

反应条件

温度
150 fahrenheit

PROCEDURE

实验过程

A styrene-butadiene-itaconic acid copolymer was prepared by adding to a pressure reactor with constant stirring 29.1 parts water, 1.0 parts itaconic acid, 0.5 parts of a 10 percent solution of Aerosol A-196 surfactant (sodium dicyclohexyl sulfosuccinate, available from American Cyanamid Co., Wayne, N.J.), and 0.5 parts of a polystyrene seed, 25 nm particle size. The mixture was heated to 150° F. and 0.2 parts sodium persulfate in 2.7 parts water was added to initiate the reaction.

WORKUP

后处理

  1. additionby adding to a pressure reactor
  2. customthe reaction