[CH2:1]=[CH:2][CH2:3][CH2:4][CH2:5][CH3:6].[CH2:7]=[CH:8][CH2:9]CCCCC.C=C>CCCCCC>[CH2:1]=[CH:2][CH2:3][CH2:4][CH2:5][CH3:6].[CH2:7]=[CH:8][CH3:9]

Participants

5

Procedure

The procedure used for the preparation of copolymer S-2 was repeated except that 1-hexene was replaced with 1 -octene. A tacky amorphous polymer was obtained in 56% conversion having an inherent viscosity of 4.2 dL/g in n-hexane and a Tg of -51° C. It contained 89 mole percent of 1-octene and 11 mole percent of ethylene.