[C:1]([O:6][CH3:7])(=[O:5])[C:2](C)=[CH2:3].[C:8](OC)(=O)[CH:9]=[CH2:10].[C:14](#[N:17])[CH:15]=[CH2:16].[CH2:18]=[CH:19][C:20]1[CH:25]=[CH:24][CH:23]=[CH:22][CH:21]=1>>[C:14](#[N:17])[CH:15]=[CH2:16].[CH2:18]=[CH:19][C:20]1[CH:25]=[CH:24][CH:23]=[CH:22][CH:21]=1.[C:1]([O:6][CH2:7][CH2:8][CH2:9][CH3:10])(=[O:5])[CH:2]=[CH2:3]

Participants

7

Procedure

Polymerization was conducted in the same manner as in Production Example 16 excepting that 36 parts of methyl methacrylate and 2 parts of methyl acrylate used in graft polymerization was changed to 10 parts of acrylonitrile and 28 parts of styrene, obtaining graft copolymer latex obtained by graft-polymerizing acrylonitrile and styrene to butyl acrylate rubber.

Workup

  1. customPolymerization
  2. customused in graft polymerization
  3. customobtaining graft copolymer

Sources & evidence

ORD record
ord-d54f9ab995a74f068ea73256fdc42e18
Source dataset
uspto-grants-2011_03
Patent number
US07910028B2

Reaction notes

Loading…