Sulfuric Acid → Sulfuric acid--prop-2-enamide (1/1)
Reaction equation
[S:1](=[O:5])(=[O:4])([OH:3])[OH:2].[C:6]([NH2:10])(=[O:9])[CH:7]=[CH2:8].N(C(C)(C)C#N)=NC(C)(C)C#N>O>[OH:4][S:1]([OH:5])(=[O:3])=[O:2].[C:6]([NH2:10])(=[O:9])[CH:7]=[CH2:8]Participants
5
Reactant 3
Product 1
Reagents, catalysts & solvents 1
Conditions
- Temperature
- 55 °C
Procedure
80 g N-(N',N',2',2'-tetramethylaminopropyl)-acrylamide was dissolved in 386 g water and acidified with 100 g 20% sulfuric acid. After addition of 100 g acrylamide, the solution was heated to 55° C. and polymerization was initiated with 80 mg azobisisobutyronitrile. After being allowed to stand for 3 hours, the gel-like copolymerization product was comminuted, dried and ground to give a white powder.
Workup
- custompolymerization
- customthe gel-like copolymerization product
- customwas comminuted
- customdried
- customto give a white powder
Sources & evidence
- ORD record
- ord-62cc5eb222754d01918fa743a5a24ac4
- Source dataset
- uspto-grants-1983_10
- Patent number
- US04408073
Reaction notes