Ammonia → Itaconic acid

HRID 716576Notes

Reaction equation

HRID 716576 reaction equation
[NH3:1].[C:2]([OH:10])(=[O:9])[C:3]([CH2:5][C:6]([OH:8])=[O:7])=[CH2:4]>CS(C)=O>[C:5](#[N:1])[CH:3]=[CH2:2].[C:2]([OH:10])(=[O:9])[C:3]([CH3:5])=[CH2:4].[C:2]([OH:10])(=[O:9])[C:3]([CH2:5][C:6]([OH:8])=[O:7])=[CH2:4]

Participants

6

Procedure

95 mol % of acrylonitrile, 3 mol % of methacrylic acid and 2 mol % of itaconic acid were polymerized by solution polymerization using dimethylsulfoxide as a solvent, and then ammonia was added thereto in an amount equivalent to that of itaconic acid to neutralize the reaction product to prepare a polyacrylontrile-based copolymer in the form of an ammonium salt, thereby obtaining a spinning solution including 22 wt % of the polyacrylontrile-based copolymer.

Workup

  1. customobtaining a spinning solution

Sources & evidence

ORD record
ord-f7ee1799bfea4315b1ba253a3883535b
Source dataset
uspto-grants-2015_11
Patent number
US09187847B2

Reaction notes