Reaktionsgleichung
[C:1]1([CH2:9]O)(C[OH:8])[CH2:6][CH2:5][CH2:4][CH2:3][CH2:2]1.[C:11](O)(=O)[C:12]1[CH:20]=[CH:19][C:15]([C:16]([OH:18])=[O:17])=[CH:14][CH:13]=1.C([O-])(=O)[C:24]1[CH:32]=[CH:31][C:27]([C:28]([O-:30])=[O:29])=[CH:26][CH:25]=1>C(O)CO>[C:20]1(=[O:8])[O:17][C:16](=[O:18])[CH:15]=[CH:19]1.[CH2:11]=[CH:9][C:1]1[CH:2]=[CH:3][CH:4]=[CH:5][CH:6]=1.[C:28]([O:30][O:18][C:16](=[O:17])[C:15]1[CH:14]=[CH:13][CH:12]=[CH:20][CH:19]=1)(=[O:29])[C:27]1[CH:31]=[CH:32][CH:24]=[CH:25][CH:26]=1Komponenten
7
Edukt 3
Produkt 3
Reagenzien, Katalysatoren, Lösungsmittel 1
Versuchsvorschrift
70 Parts by weight of a powdery polyphenylene sulfide resin (Tohpren T-4 produced by Tohpren Co., Ltd ; average particle size, 50 μm), 30 parts by weight of a polyester composed of cyclohexanedimethanol and terephtalic acid (polycyclohexanedimethylene terephthalate (hereinafter referred to as PCT); [η]=0.9), which is a thermopalstic polyester, 12 parts by weight of an unsaturated polyester obtained from ethylene glycol and maleic acid anhydride ([η]=0.2), 6 parts by weight of styrene and 1 part by weight of benzoyl peroxide were mixed. The mixture was extruded through a twin-screw extruder (Werner Pfleiderer 30 Φ) at a barrel temperature of 30° C. and pelletized on a pelletizer.
Quellen und Nachweise
- ORD-Eintrag
- ord-9adf36a9793a44ce816bbbf330cfa4d0
- Quelldatensatz
- uspto-grants-1991_03
- Patentnummer
- US04997866
Verknüpfte Notizen