O.[CH2:2]([OH:5])[CH2:3][OH:4].CCCCC(CC[CH:15]([O:20]S([O-])(=O)=O)CC(C)C)CC.[Na+]>[Cu]=O.[O-2].[Zr+4].[O-2].OCC(CO)O>[CH2:2]([OH:5])[CH2:3][OH:4].[OH:4][CH2:3][CH:2]([CH2:15][OH:20])[OH:5]A copper oxide dispersion was produced by mixing 2.0 g NanoArc® copper oxide, 4.9 g deionized water, 0.10 g PVP K-30, 0.5 g ethylene glycol, 0.03 g Tergitol® TMN-6, 0.01 g Dynol® 604, and 1.32 g glycerol in a 20 mL vial. 5 g of zirconium oxide milling media was added and the vial was agitated for 60 minutes.