反応式
[C:1]([O:5][C:6](=[O:9])[CH:7]=[CH2:8])([CH3:4])([CH3:3])[CH3:2].[C:10]([OH:14])(=[O:13])[CH:11]=[CH2:12].[C:15]([O:20][CH2:21][CH2:22][CH2:23][OH:24])(=[O:19])[C:16]([CH3:18])=[CH2:17].CC(OC(C)=O)COC>CC(N=NC(C#N)(C)C)(C#N)C>[C:6]([O:5][C:1]([CH3:4])([CH3:3])[CH3:2])(=[O:9])[CH:7]=[CH2:8].[C:10]([OH:14])(=[O:13])[CH:11]=[CH2:12].[C:15]([O:20][CH2:21][CH2:22][CH2:23][OH:24])(=[O:19])[C:16]([CH3:18])=[CH2:17]参加物
6
実験手順
10 g of t-butylacrylate, 4 g of acrylic acid, 6 g of 3-hydroxypropyl methacrylate and 0.4 g of AIBN were added to 200 g of PGMEA, and were then polymerized at 60° C. for 8 hours. After completion of the polymerization, the mixture was precipitated in ether, filtered, and dried in vacuo to yield 17 g of t-butyl acrylate-acrylic acid-3-hydroxypropyl methacrylate copolymer, as a white solid, represented by Formula 2 below:
後処理
- customwere then polymerized at 60° C. for 8 hours
- customAfter completion of the polymerization
- customthe mixture was precipitated in ether
- filtrationfiltered
- customdried in vacuo
出典と根拠
- ORDレコード
- ord-eb8c73245c1e4136871d0a3dd29432be
- 出典データセット
- uspto-grants-2006_12
- 特許番号
- US07147994B2