HRID1920607

反应详情

EQUATION

反应方程式

HRID 1920607 的结构方程式

AUXILIARIES

试剂、催化剂与溶剂

2

PROCEDURE

实验过程

The following composition was prepared. The polymer solution was composed of 50% by weight of poly(lactide-co-glycolide) (PLGH) with a lactide to glycolide ratio of 75/25 and with an inherent viscosity of 0.20 dL/g dissolved in 50% by weight N-methyl-2-pyrrolidone. The active portion was composed of GHRP-1 and citric acid. The ratio of citric acid to GHRP-1 was about 1.25:1 on a molar basis. The GHRP-1 was dissolved in water; citric acid was added to dissolve; and the solution was filled into a syringe and lyophilized. The contents of the completed syringe were about 80 mg of GHRP-1 and about 20 mg of citric acid.

WORKUP

后处理

  1. customThe following composition was prepared
  2. dissolutionto dissolve
  3. additionand the solution was filled into a syringe