Sulfuric Acid → Benzene, ethenyl-, polymer with 1,3-butadiene

HRID 460400

反応式

HRID 460400 の反応式
[CH2:1]=[CH:2][CH:3]=[CH2:4].[CH2:5]=[CH:6][C:7]1[CH:12]=[CH:11][CH:10]=[CH:9][CH:8]=1.C([O-])(=O)CCCCCCC/C=C\CCCCCCCC.[K+].O=C[C@@H]([C@H]([C@@H]([C@@H](CO)O)O)O)O.[O-]P(OP([O-])([O-])=O)(=O)[O-].[Na+].[Na+].[Na+].[Na+].S(=O)(=O)(O)O>O>[CH2:1]=[CH:2][CH:3]=[CH2:4].[CH2:5]=[CH:6][C:7]1[CH:12]=[CH:11][CH:10]=[CH:9][CH:8]=1

参加物

8

実験手順

50 parts of butadiene rubber latex powder, 50 parts of styrene and 150 parts of deionized water were blended. To the blend, 1.0 parts of potassium oleate, 0.4 parts of cumenhydroperoxide, 0.2 parts of mercaptan-containing chain transfer agent, 0.4 parts of glucose, 0.01 parts of ferrous sulfate hydrate, and 0.3 parts of sodium pyrophosphate were added. The blend was kept at 75° C. for 5 hours to obtain g-ABS latex. To the g-ABS latex, 0.4 parts of sulfuric acid was added, coagulated and dried to obtain butadiene-styrene graft copolymer resin (g-BS) in a powder form.

後処理

  1. additionwere added
  2. customto obtain g-ABS latex
  3. customdried

出典と根拠

ORDレコード
ord-6c240420062249dfb41ba0ba3e9b74eb
出典データセット
uspto-grants-2007_03
特許番号
US07196126B2

関連ノート

読み込み中…